I'm at the final few finishs of my cigarbox uke. I sanded then applied tungoil high gloss. I steel wooled between finishes with 0000 steel wool. I wet sanded last night with 600 grit and put the 6th coat on tonight and it's starting to look good. I have a few questions. Am I going at it the right way with the steel wool between coats and also I'm waiting 24 hours between coats? How many more coats will it require? What do I do after the final coat drys? Do I wet sand with the 600 lightly just enough to scuff it up a little and then polish it out with something like minwax? Thanks for taking the time to read this and I know these are probably dumb questions but I just don't know.